Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FLEX NORYL™ Resin WCP921A - Asia - (PPE+TPE) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for FLEX NORYL™ Resin WCP921A - Asia:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Flex Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
FLEX NORYL™ WCP921A resin is a flexible, non-reinforced injection moldable blend of Polyphenylene Ether (PPE) + Styrene Ethylene Butylene Styrene (SEBS) + Polyolefin. This material contains non-halogenated flame retardant and carries a UL94 flame rating of V0 at 6mm. FLEX NORYL WCP921A resin is intended for evaluation in over-molding applications such as plugs, strain reliefs, and connectors. It has a Shore A Hardness reading of 92 and exhibits low specific gravity, very low water absorption, and dimensional stability.

UL Yellow Card Link E207780-100886805
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Indice di fluidità a caldo, MFI 10 g/10min ASTM D 1238
Temperatura 250 °C -
Carico 2.16 kg -
Ritiro di stampaggio, parallelo 0.4 mm/mm ASTM D 955
Ritiro di stampaggio, perpend. 0.4 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Carico unitario a rottura 9 MPa ISO 527
Deformazione a rottura 50 % ISO 527
ASTM Data
Resistenza alla trazione a rottura 9 MPa ASTM D 638
Allungamento a rottura 120 % ASTM D 638
Durezza A Shore 92 - ASTM D 2240
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Reazione al fuoco a spessore h V-0 class IEC 60695-11-10
Spessore provato 6.0 mm -
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (2) 3 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 2.8 - IEC 62631-2-1
Fattore di dissipazione, 1MHz 60 E-4 IEC 62631-2-1
Res. Alle correnti striscianti superficiali 600 - IEC 60112
ASTM Data
Resistenza di volume >1E15 Ohm*cm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Densità 1040 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 60 - 80 °C -
Pre-essiccamento - Tempo 4 - 6 h -
Umidità del Processo ≤0.01 % -
Temperatura di fusione 220 - 250 °C -
Temperatura dello stampo 40 - 60 °C -
Zona 1 180 - 220 °C -
Zona 2 210 - 240 °C -
Zona 3 220 - 250 °C -
Velocità di Rotazione della Vite 30 - 80 rpm -
Contropressione 3 - 10 MPa -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Additivi
Agente ritardante di fiamma
Caratteristiche speciali
Ritardante di fiamma
Disponibilità geografica
Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.